After a ton of mahogany wood is made into furniture, there are only six hundred kilograms left, and the remaining 1400 kilograms of wood are actually consumed in the production process. Yes, that is the case.
Solid wood furniture has become more and more concerned with the popularity of wenwan in recent years. Solid wood furniture has high requirements for logs, not only the stability of wood, but also a larger part of the requirements for log caliber.
Let's count the bill:
After the logs are polished, the loss of moisture is 15%, the average loss of the flat saw is 8%, the loss of planing is 8%, the loss of engraving is 18%, and the loss of splitting damage is 20%. The actual utilization rate is only 31%. %.
A lot of wood chips are produced during the wood cutting process, and most of these wood chips are wasted as garbage, which is said to account for as much as eight percent of the wood!
Then the problem of the wood itself, the wood can not be perfect, cut white skin, insect eyes, rotten heart according to demand, every piece of wood is not necessarily, on average, it will waste nearly 20%!
The mahogany wood used to make furniture needs to be dried. After drying, the moisture loss is about 15%. Under normal circumstances, it should be dried for about three times.
The enamel process in the mahogany: smashing eyes, hoeing, wood cutting adjustment, etc., inevitably produce a batch of wood chips and trim.
In the process of engraving, it is necessary to waste 18%. Before painting, it needs to be scraped. All kinds of utensils are scraped against the wood until the furniture is flat and natural, and then polished and polished to make it more delicate. It is also a waste of wood.
After finishing the lacquer, the mahogany furniture is completely finished, and finally it needs to be dried for 20-25 days in order to face the consumers, which will remove some moisture and lose weight. Just one thousand four hundred pounds disappeared!
The solid wood slab looks unpretentious, but the production process is quite grueling. The raw wood produced also needs to bear a lot of risks. There is no hollow inside the logs, the wood grain is not enough enough, and any small detail may damage the solid wood slab. The overall effect.
These interlocking manual processes are probably one of the charms of solid wood slabs. Finally, put some solid wood slabs in the factory together to enjoy.
Hair extension keratin glue granules can be applied with fusion iron connector, hair extension iron, pre-bonding hair, good for hair extension or nail extension, the abundant quantity is enough for you to use and replace.
Strong keratin granule beads have nice viscosity, they have strong adhesion effect, there is no carbonation in continuous use, aging resistance, less wire drawing, no odor, safe for you to use
these granule beads are made from quality EVA, which are safe for use on the hair, they can melt and flow at high temperatures of 270 to 340 degrees Fahrenheit, you can use our product to create various hair styles
Hot melt glue stick suitable for Human Hair Works well in all temperatures.Can be used with Hair Extension Glue Gun & pre-bonding Hair Extension.
hot glue sticks fits most of glue guns on the market. It's also incredibly durable, flexible and long lasting. Good flexibility and luster, durability for daily gluing .
Hot fusion extensions tools are good for bonding heat-sensitive materials, not only can be applied for grafted wig, but also for nail extension, manual, accessories, shoes, wood products, ceramics, toys, cardboard boxes and more
Solid Glue,Italian Keratin Glue Grains,Keratin Glue Granule Bead,Hot Melt Glue Stick For Hair Extension
Xuchang Le Yi De Import And Export Trade Co., Ltd. , https://www.synthetichairs.com